Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | BrO3TS12S5 ( БрО3Ц12С5 ) ( БрОЦС3-12-5 ) |
Classification : | Tin foundry bronzes |
Equivalent grades: | Go here |
Fe | Si | P | Al | Cu | Pb | Zn | Sb | Sn | Impurity | - |
max 0.4 | max 0.02 | max 0.05 | max 0.02 | 74.2 - 87 | 3 - 6 | 8 - 15 | max 0.5 | 2 - 3.5 | all 1.3 | Si + Al < 0.02 % |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar, GOST 24301-93 | 180-220 | 16-20 | ||||||
cast in a metal mould, GOST 613-79 | 206 | 5 | ||||||
sand (mould) casting, GOST 613-79 | 176 | 8 |
Brinell hardness for BrO3TS12S5 ( БрО3Ц12С5 ) , Bar GOST 24301-93 | HB 10 -1 = 60 - 65 MPa |
Brinell hardness for BrO3TS12S5 ( БрО3Ц12С5 ) , cast in a metal mould GOST 613-79 | HB 10 -1 = 60 MPa |
Brinell hardness for BrO3TS12S5 ( БрО3Ц12С5 ) , sand (mould) casting GOST 613-79 | HB 10 -1 = 60 MPa |
Melting temperature : | 998 °C |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.823 | 8700 |
USA | Japan | |||
- | JIS | |||
|
|
B55 - Bars |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)