Grade : | BrO6TS6S3 ( БрО6Ц6С3 ) |
Classification : | Tin foundry bronzes |
Equivalent grades: | Is absent |
Fe | Si | P | Al | Cu | Pb | Zn | Sb | Sn | Impurity |
max 0.4 | max 0.02 | max 0.05 | max 0.05 | 80.7 - 88 | 2 - 4 | 5 - 7 | max 0.5 | 5 - 7 | all 1.3 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
cast in a metal mould, GOST 613-79 | 176 | 4 | Without heat treatment | |||||
sand (mould) casting, GOST 613-79 | 147 | 6 | Without heat treatment |
Brinell hardness for BrO6TS6S3 ( БрО6Ц6С3 ) (without heat treatment) , GOST 613-79 | HB 10 -1 = 60 MPa |
Melting temperature : | 967 °C |
Casting temperature : | 1150 °C |
Linear shrinkage : | 1.6 % |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.882 | 17.1 | 75.4 | 8820 | 90 |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |