Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Bronze

Characteristics for grade     BrO8TS4   ( БрО8Ц4 )



      Grade :     BrO8TS4   ( БрО8Ц4 )
      Classification :   Tin foundry bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrO8TS4   ( БрО8Ц4 )
Fe Si PAl Cu PbZn Sb Sn Impurity -
max   0.3max   0.02max   0.05max   0.0284 - 89max   0.54 - 6max   0.37 - 9 all 1 Si + Al < 0.02 %
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrO8TS4   ( БрО8Ц4 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 613-79     196   10   Without heat treatment
sand (mould) casting, GOST 613-79     196   10   Without heat treatment


    Brinell hardness for     BrO8TS4   ( БрО8Ц4 )   (without heat treatment) ,       GOST 613-79 HB 10 -1 = 75   MPa


Friction coefficient of the material   BrO8TS4   ( БрО8Ц4 ) .
 Friction coefficient with oil : 0.006
 Friction coefficient without oil : 0.3


Technological properties of the material   BrO8TS4   ( БрО8Ц4 ) .
        Melting temperature : 1000   °C
        Casting temperature : 1100 - 1150   °C
        Linear shrinkage : 1.47   %


Physical properties for grade   BrO8TS4   ( БрО8Ц4 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.98 16.6 68.2 8800 356 135


Equivalent steels for grade     BrO8TS4   ( БрО8Ц4 )
Warning! Indicated both exact and nearest equivalents.
USA
-
C90300




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrO8TS4   ( БрО8Ц4 ) - Tin foundry bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru