Characteristics for grade     BrO10F1   ( БрО10Ф1 )



      Grade :     BrO10F1   ( БрО10Ф1 )
      Classification :   Tin foundry bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrO10F1   ( БрО10Ф1 )
Fe Si PAl Cu PbZn Sb Sn Impurity
max   0.2max   0.020.4 - 1.1max   0.0286.9 - 90.6max   0.3max   0.3max   0.39 - 11 all 1
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrO10F1   ( БрО10Ф1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 613-79     245   3   Without heat treatment
sand (mould) casting, GOST 613-79     215   3   Without heat treatment


    Brinell hardness for     BrO10F1   ( БрО10Ф1 )   (without heat treatment) ,     cast in a metal mould GOST 613-79 HB 10 -1 = 90   MPa
    Brinell hardness for     BrO10F1   ( БрО10Ф1 )   (without heat treatment) ,     sand (mould) casting GOST 613-79 HB 10 -1 = 80   MPa


Friction coefficient of the material   BrO10F1   ( БрО10Ф1 ) .
 Friction coefficient with oil : 0.008
 Friction coefficient without oil : 0.15
 Friction coefficient in sea : 0.37


Technological properties of the material   BrO10F1   ( БрО10Ф1 ) .
        Melting temperature : 934   °C
        Linear shrinkage : 1.44   %


Physical properties for grade   BrO10F1   ( БрО10Ф1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.03 17   8760    


Equivalent steels for grade     BrO10F1   ( БрО10Ф1 )
Warning! Indicated both exact and nearest equivalents.
GermanyEnglandEuropeanPolandCzechiaInter
DIN,WNrBSEN PNCSNISO
CuSn10P
PB1
CC481K
CuSn11P-C
CuSn10P
423120
CuSn10P



Types of delivery of grade   BrO10F1   ( БрО10Ф1 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrO10F1   ( БрО10Ф1 ) - Tin foundry bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru