Characteristics for grade     BrO10TS2   ( БрО10Ц2 )



      Grade :     BrO10TS2   ( БрО10Ц2 )
      Classification :   Tin foundry bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrO10TS2   ( БрО10Ц2 )
Fe Si PAl Cu PbZn Sb Sn Impurity -
max   0.3max   0.02max   0.05max   0.0285 - 90max   0.51 - 3max   0.39 - 11 all 1 Si + Al < 0.02 %
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrO10TS2   ( БрО10Ц2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 613-79     225   10   Without heat treatment
sand (mould) casting, GOST 613-79     215   10   Without heat treatment


    Brinell hardness for     BrO10TS2   ( БрО10Ц2 )   (without heat treatment) ,     cast in a metal mould GOST 613-79 HB 10 -1 = 75   MPa
    Brinell hardness for     BrO10TS2   ( БрО10Ц2 )   (without heat treatment) ,     sand (mould) casting GOST 613-79 HB 10 -1 = 65   MPa


Friction coefficient of the material   BrO10TS2   ( БрО10Ц2 ) .
 Friction coefficient with oil : 0.034
 Friction coefficient without oil : 0.18


Technological properties of the material   BrO10TS2   ( БрО10Ц2 ) .
        Melting temperature : 1015   °C
        Casting temperature : 1120 - 1150   °C
        Linear shrinkage : 1.48   %


Physical properties for grade   BrO10TS2   ( БрО10Ц2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.98 17.3 55.3 8500 381 155


Equivalent steels for grade     BrO10TS2   ( БрО10Ц2 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanEnglandItalySwedenPolandCzechia
-DIN,WNrJIS BSUNISSPNCSN
C90500
2.1087
GCuSn10Zn
Rg10
BC3
B1
GCuSn10Zn2
CuSn10Zn2
CuSn10Zn2
423138




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrO10TS2   ( БрО10Ц2 ) - Tin foundry bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru