Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | LO62-1 ( ЛО62-1 ) |
Classification : | Copper-zinc alloys pressure treated |
Equivalent grades: | Go here |
Fe | P | Cu | Pb | Zn | Sb | Bi | Sn | Impurity |
max 0.1 | max 0.01 | 61 - 63 | max 0.1 | 35.6 - 38.3 | max 0.005 | max 0.002 | 0.7 - 1.1 | all 0.3 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar, GOST 2060-2006 | 390 | |||||||
Bar, GOST 2060-2006 | 360 | |||||||
Strip hotrolled, GOST 931-90 | 340-440 | 20 | ||||||
Strip, GOST 931-90 | 390 | 5 |
Brinell hardness for LO62-1 ( ЛО62-1 ) , Sheet GOST 2208-2007 | HB 10 -1 = 145 MPa |
Brinell hardness for LO62-1 ( ЛО62-1 ) , Bar GOST 2060-2006 | HB 10 -1 = 100 MPa |
Brinell hardness for LO62-1 ( ЛО62-1 ) , Bar GOST 2060-2006 | HB 10 -1 = 80 MPa |
Melting temperature : | 906 °C |
Forging temperature : | 700 - 780 °C |
Annealing temperature : | 550 - 650 °C |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 1.05 | 108.9 | 8500 | 78 | ||
100 | 19.3 |
USA | Germany | Japan | |||||
- | DIN,WNr | JIS | |||||
|
|
|
B53 - Sheets and Strips |
В54 - Ribbons |
B55 - Bars |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)