Characteristics for grade     LS60-1   ( ЛС60-1 )



      Grade :     LS60-1   ( ЛС60-1 )
      Classification :   Copper-zinc alloys pressure treated
      Equivalent grades:   Go here



Chemical composition in % for grade   LS60-1   ( ЛС60-1 )
Fe P Cu PbZn Sb Bi Impurity
max   0.15max   0.0159 - 610.6 - 137.5 - 40.4max   0.005max   0.002 all 0.5
Comment: Zn is a basis; the percentage of Zn is given approximately.


Mechanical properties under Т=20oС for grade   LS60-1   ( ЛС60-1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
soft     300-400  45-55   
hard     600-700  4-6   


    Brinell hardness for     LS60-1   ( ЛС60-1 )   ,     soft HB 10 -1 = 60 - 70   MPa
    Brinell hardness for     LS60-1   ( ЛС60-1 )   ,     hard HB 10 -1 = 150 - 160   MPa


Friction coefficient of the material   LS60-1   ( ЛС60-1 ) .
 Friction coefficient with oil : 0.1
 Friction coefficient without oil : 0.22


Technological properties of the material   LS60-1   ( ЛС60-1 ) .
        Melting temperature : 900   °C
        Annealing temperature : 600 - 650   °C


Physical properties for grade   LS60-1   ( ЛС60-1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.05     8500   65
100   20.8        


Equivalent steels for grade     LS60-1   ( ЛС60-1 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySwedenCzechiaInter
-DIN,WNrJIS AFNORBSEN UNISSCSNISO
C36500
2.0372
CuZn39Pb0.5
C3710
C3712
CuZn39Pb0.8
CZ123
CuZn37Pb1
CW605N
PCuZn39Pb1
CuZn40Pb
423221
CuZn37Pb1




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  LS60-1   ( ЛС60-1 ) - Copper-zinc alloys pressure treated: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru