Characteristics for grade     LS59-1   ( ЛС59-1 )



      Grade :     LS59-1   ( ЛС59-1 )
      Classification :   Copper-zinc alloys pressure treated
      Equivalent grades:   Go here



Chemical composition in % for grade   LS59-1   ( ЛС59-1 )
Fe P Cu PbZn Sb Bi Sn Impurity -
max   0.5max   0.0257 - 600.8 - 1.937.05 - 42.2max   0.01max   0.003max   0.3 all 0.75 Si + Sn < 0.5 %
Comment: Zn is a basis; the percentage of Zn is given approximately.


Mechanical properties under Т=20oС for grade   LS59-1   ( ЛС59-1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 494-90     390        
Bar, GOST 2060-2006     360   22    
Bar, GOST 31366-2008     490   7    
Bar, GOST 31366-2008     330   25    
Wire, GOST 1066-90     340   25-30   
Wire, GOST 1066-90     440-640  1-8   
Strip, GOST 931-90     460-610  5    
Strip, GOST 931-90     340-470  25    
Strip hotrolled, GOST 931-90     360-490  18    


    Brinell hardness for     LS59-1   ( ЛС59-1 )   ,     Sheet GOST 2208-2007 HB 10 -1 = 100   MPa
    Brinell hardness for     LS59-1   ( ЛС59-1 )   ,     Sheet GOST 2208-2007 HB 10 -1 = 200   MPa
    Brinell hardness for     LS59-1   ( ЛС59-1 )   ,     Bar GOST 2060-2006 HB 10 -1 = 80   MPa
    Brinell hardness for     LS59-1   ( ЛС59-1 )   ,     Bar GOST 2060-2006 HB 10 -1 = 130   MPa


Friction coefficient of the material   LS59-1   ( ЛС59-1 ) .
 Friction coefficient with oil : 0.0135
 Friction coefficient without oil : 0.17


Technological properties of the material   LS59-1   ( ЛС59-1 ) .
        Melting temperature : 900   °C
        Forging temperature : 780 - 820   °C
        Annealing temperature : 600 - 650   °C


Physical properties for grade   LS59-1   ( ЛС59-1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.05   104.7 8400   66
100   20.6     376.8  


Equivalent steels for grade     LS59-1   ( ЛС59-1 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanEnglandEuropeanPolandCzechiaAustriaInter
-DIN,WNrJIS BSEN PNCSNONORMISO
C37000
C38000
2.0402
CuZn38Pb1.5
CuZn40Pb2
C3710
CZ129
CuZn38Pb1
CW607N
CuZn38Pb1.5
423222
CuZn38Pb1
CuZn39Pb1



Types of delivery of grade   LS59-1   ( ЛС59-1 )
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  LS59-1   ( ЛС59-1 ) - Copper-zinc alloys pressure treated: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru