Grade : | LTS40Mts1.5 ( ЛЦ40Мц1.5 ) ( ЛМц58-2Л ) |
Classification : | Cast cooper-zinc alloys |
Equivalent grades: | Is absent |
Fe | Si | Mn | Ni | P | Cu | Pb | Zn | Sb | Sn | Impurity |
max 1.5 | max 0.1 | 1 - 2 | max 1 | max 0.03 | 57 - 60 | max 0.7 | 36 - 42 | max 0.1 | max 0.5 | all 2 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
cast in a metal mould, GOST 17711-93 | 392 | 20 | ||||||
sand (mould) casting, GOST 17711-93 | 372 | 20 | ||||||
centrifugal casting, GOST 17711-93 | 392 | 20 |
Brinell hardness for LTS40Mts1.5 ( ЛЦ40Мц1.5 ) , cast in a metal mould GOST 17711-93 | HB 10 -1 = 110 MPa |
Brinell hardness for LTS40Mts1.5 ( ЛЦ40Мц1.5 ) , sand (mould) casting GOST 17711-93 | HB 10 -1 = 100 MPa |
Brinell hardness for LTS40Mts1.5 ( ЛЦ40Мц1.5 ) , centrifugal casting GOST 17711-93 | HB 10 -1 = 110 MPa |
Friction coefficient with oil : | 0.012 |
Friction coefficient without oil : | 0.32 |
Melting temperature : | 880 °C |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 21.2 | 71.2 | 8400 | 108 |
B51 - Non-ferrous metals, including rare metals, and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |