Characteristics for grade     BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )



      Grade :   BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 ) (   CuA110Fe3Mn1   )
      Classification :   Tin-free pressure-worked bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )
Fe Si Mn PAl Cu PbZn Sn Impurity
2 - 4max   0.11 - 2max   0.019 - 1182.3 - 88max   0.03max   0.5max   0.1 all 0.7
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 1208-90     540-590  12    
Bar, GOST 1628-78     590   12    


    Brinell hardness for     BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )   ,     Pipe GOST 1208-90 HB 10 -1 = 129 - 200   MPa
    Brinell hardness for     BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )   ,     Bar GOST 1628-78 HB 10 -1 = 130 - 200   MPa


Friction coefficient of the material   BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 ) .
 Friction coefficient with oil : 0.012
 Friction coefficient without oil : 0.21


Technological properties of the material   BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 ) .
        Melting temperature : 1045   °C
        Forging temperature : 750 - 850   °C
        Annealing temperature : 650 - 750   °C


Physical properties for grade   BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1   80 7500   190
100   16.1        


Equivalent steels for grade     BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )
Warning! Indicated both exact and nearest equivalents.
GermanyEuropeanPolandCzechiaAustriaInter
DIN,WNrEN PNCSNONORMISO
2.0936
CuAI10Fe3Mn3
CuAl10Fe3Mn2
CuAI10Fe3Mn2
CuAI10Fe3Mn2
423046
CuAI10Fe3Mn2
CuAI10Fe3



Types of delivery of grade   BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 )
В05 - Welding and cutting of metals., Soldering, riveting
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrАZHMts10-3-1.5   ( БрАЖМц10-3-1.5 ) - Tin-free pressure-worked bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru