Characteristics for grade     BrАZHN10-4-4   ( БрАЖН10-4-4 )



      Grade :   BrАZHN10-4-4   ( БрАЖН10-4-4 ) (   CuA110Fe4Ni4   )
      Classification :   Tin-free pressure-worked bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrАZHN10-4-4   ( БрАЖН10-4-4 )
Fe Si Mn Ni PAl Cu PbZn Sn Impurity
3.5 - 5.5max   0.1max   0.33.5 - 5.5max   0.019.5 - 1177.4 - 83.5max   0.02max   0.3max   0.1 all 0.6
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrАZHN10-4-4   ( БрАЖН10-4-4 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 1208-90     640   5    
Bar, GOST 1628-78     640   5    


    Brinell hardness for     BrАZHN10-4-4   ( БрАЖН10-4-4 )   ,     Pipe GOST 1208-90 HB 10 -1 = 170 - 220   MPa
    Brinell hardness for     BrАZHN10-4-4   ( БрАЖН10-4-4 )   ,     Bar GOST 1628-78 HB 10 -1 = 170 - 220   MPa


Friction coefficient of the material   BrАZHN10-4-4   ( БрАЖН10-4-4 ) .
 Friction coefficient with oil : 0.011
 Friction coefficient without oil : 0.23


Technological properties of the material   BrАZHN10-4-4   ( БрАЖН10-4-4 ) .
        Melting temperature : 1084   °C
        Forging temperature : 800 - 900   °C
        Annealing temperature : 700 - 750   °C


Physical properties for grade   BrАZHN10-4-4   ( БрАЖН10-4-4 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.15   80 7500   190
100   17.1        


Equivalent steels for grade     BrАZHN10-4-4   ( БрАЖН10-4-4 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyPolandCzechiaAustriaInter
-DIN,WNrJIS AFNORBSEN UNIPNCSNONORMISO
C63000
2.0966
CuAl10Ni5Fe4
C6301
CuAI9Ni5Fe3
CA104
CuAI10Ni5Fe4
PCuAI10Fe5Ni5
CuAI10Ni5Fe4
423047
CuAI10Ni5Fe4
CuAI10Ni5Fe4



Types of delivery of grade   BrАZHN10-4-4   ( БрАЖН10-4-4 )
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrАZHN10-4-4   ( БрАЖН10-4-4 ) - Tin-free pressure-worked bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru