Grade : | BrOTS4-3 ( БрОЦ4-3 ) |
Classification : | Wrought tin bronzes |
Equivalent grades: | Is absent |
Fe | Si | Ni | P | Al | Cu | Pb | Zn | Sb | Bi | Sn | Impurity |
max 0.05 | max 0.002 | max 0.3 | max 0.03 | max 0.002 | 92.2 - 93.8 | max 0.02 | 2.7 - 3.3 | max 0.002 | max 0.002 | 3.5 - 4 | all 0.2 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar, GOST 10025-78 | Ø 42 - 120 | 270 | 35 | |||||
Bar, GOST 10025-78 | Ø 5 - 40 | 310-430 | 12-20 | |||||
Wire, GOST 5221 - 2008 | 760-880 | 0.5-2 | ||||||
Strip, GOST 1789-70 | 290 | 110 | 35-38 | |||||
Strip, GOST 1789-70 | 540-690 | 510-670 | 2-4 |
Brinell hardness for BrOTS4-3 ( БрОЦ4-3 ) , soft | HB 10 -1 = 50 - 70 MPa |
Brinell hardness for BrOTS4-3 ( БрОЦ4-3 ) , hard | HB 10 -1 = 150 - 170 MPa |
Melting temperature : | 1045 °C |
Forging temperature : | 700 - 800 °C |
Annealing temperature : | 550 - 650 °C |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 1.22 | 84 | 8800 | 90 | ||
100 | 18 |
В05 - Welding and cutting of metals., Soldering, riveting |
B53 - Sheets and Strips |
B55 - Bars |
B74 - Wire made of non-ferrous metals and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |