Characteristics for grade     АSM   ( АСМ )



      Grade :     АSM   ( АСМ )
      Classification :   Alluminium antifriction alloys
      Equivalent grades:     Is absent



Chemical composition in % for grade   АSM   ( АСМ )
Fe Si Mn Al Cu Mg Zn Sb Impurity
max   0.75max   0.5max   0.291.05 - 96.2max   0.10.3 - 0.7max   0.13.5 - 6.5 other 0.1
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   АSM   ( АСМ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
      85-9532-4630-3845-52  


    Brinell hardness for     АSM   ( АСМ )   (hot-rolled, annealing) ,       HB 10 -1 = 22 - 26   MPa
    Brinell hardness for     АSM   ( АСМ )   (annealing) ,     Strip HB 10 -1 = 22 - 30   MPa


Limiting operating condition of the material   АSM   ( АСМ )
Load Speed Load * Speed Temperature
MPa m/s MPa * m/s Grade
19.510   100


Physical properties for grade   АSM   ( АСМ )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2830    




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АSM   ( АСМ ) - Alluminium antifriction alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru