Grade : | M1r ( М1р ) |
Classification : | Copper |
Equivalent grades: | Go here |
Fe | Ni | S | P | As | Pb | Zn | O | Sb | Bi | Sn | - |
max 0.005 | max 0.002 | max 0.005 | 0.002 - 0.012 | max 0.002 | max 0.005 | max 0.005 | max 0.01 | max 0.002 | max 0.001 | max 0.002 | Cu+Ag min 99.9 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe, GOST 617-2006 | 180-190 | 32 | ||||||
Pipe, GOST 21646-2003 | 200 | 35 | ||||||
Pipe, GOST 21646-2003 | 290 | 3 | ||||||
soft cold-rolled, GOST 1173-2006 | 200-260 | 42 | ||||||
hard cold-rolled, GOST 1173-2006 | 290 | 6 |
Brinell hardness for M1r ( М1р ) , soft GOST 1173-2006 | HB 10 -1 = 55 MPa |
Brinell hardness for M1r ( М1р ) , hard GOST 1173-2006 | HB 10 -1 = 95 MPa |
Melting temperature : | 1083 °C |
Casting temperature : | 1150 - 1250 °C |
Linear shrinkage : | 2.1 % |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 1.28 | 387 | 8940 | 390 | 17.8 | |
100 | 1.32 | 16.7 |
USA | Germany | Japan | European | |||||||
- | DIN,WNr | JIS | EN | |||||||
|
|
|
|
В05 - Welding and cutting of metals., Soldering, riveting |
B51 - Non-ferrous metals, including rare metals, and their alloys |
B53 - Sheets and Strips |
В54 - Ribbons |
B55 - Bars |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |