Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     А20   ( А20 )

      Grade :     А20   ( А20 )
      Substitute:   А12
      Classification :   Rolled steel of improved and high cutting machinability
      Equivalent grades:   Go here



Chemical composition in % for grade   А20   ( А20 )
C Si Mn S P Cu
0.17 - 0.250.15 - 0.350.7 - 10.08 - 0.15max   0.06max   0.25


Temperature of critical points for grade   А20   ( А20 ).
Ac1 = 735 ,      Ac3(Acm) = 866 ,       Ar3(Arcm) = 840 ,       Ar1 = 685


Mechanical properties under Т=20oС for grade   А20   ( А20 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Rolled stock hotrolled, GOST 1414-75     450   20 30  
Rolled stock, GOST 1414-75     530   7    


    Brinell hardness for     А20   ( А20 )   ,     Rolled stock GOST 1414-75 HB 10 -1 = 168   MPa
    Brinell hardness for     А20   ( А20 )   ,     Rolled stock GOST 1414-75 HB 10 -1 = 217   MPa


Technological properties for grade   А20   ( А20 )
  Weldability: is not used.
 Flakes : predisposed
Temper brittleness: not predisposed


Equivalent steels for grade     А20   ( А20 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyFranceChinaBulgariaRomaniaCzechia
-DIN,WNrAFNORGBBDSSTASCSN
1120
G11170
22S20
22SPb20
20F2
Y20
A20
AUT20
11120

Types of delivery of grade   А20   ( А20 )
В22 - Graded and shaped rolling
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  А20   ( А20 ) - Rolled steel of improved and high cutting machinability: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com