Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Bronze

Characteristics for grade     BrА9ZH3L   ( БрА9Ж3Л )



      Grade :   BrА9ZH3L   ( БрА9Ж3Л ) (   БрАЖ9-4Л   )
      Classification :   Tin-free foundary bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrА9ZH3L   ( БрА9Ж3Л )
Fe Si Mn Ni PAl Cu As PbZn Sb Sn Impurity
2 - 4max   0.2max   0.5max   1max   0.18 - 10.582.8 - 90max   0.05max   0.1max   1max   0.05max   0.2 all 2.7
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrА9ZH3L   ( БрА9Ж3Л )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 493-79     490   12    
sand (mould) casting, GOST 493-79     392   10    


    Brinell hardness for     BrА9ZH3L   ( БрА9Ж3Л )   ,     cast in a metal mould GOST 493 HB 10 -1 = 100   MPa
    Brinell hardness for     BrА9ZH3L   ( БрА9Ж3Л )   ,     sand (mould) casting GOST 493 HB 10 -1 = 100   MPa


Friction coefficient of the material   BrА9ZH3L   ( БрА9Ж3Л ) .
 Friction coefficient with oil : 0.004
 Friction coefficient without oil : 0.18


Physical properties for grade   BrА9ZH3L   ( БрА9Ж3Л )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.2 16 58.6 7600   110


Equivalent steels for grade     BrА9ZH3L   ( БрА9Ж3Л )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySwedenPolandCzechia
-DIN,WNrJIS AFNORBSEN UNISSPNCSN
C95200
C95400
2.0941
FeAlBz
GCuAI10Fe
AIBC1
H5114/class1
CuAI10Fe3
AB1
CuAI10Fe2-C
GCuAI10Fe3
CuAI10Fe3
CuAI10Fe3
423145




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrА9ZH3L   ( БрА9Ж3Л ) - Tin-free foundary bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru