Characteristics for grade     BrА10ZH3Mts2   ( БрА10Ж3Мц2 )



      Grade :     BrА10ZH3Mts2   ( БрА10Ж3Мц2 )
      Classification :   Tin-free foundary bronzes
      Equivalent grades:     Is absent



Chemical composition in % for grade   BrА10ZH3Mts2   ( БрА10Ж3Мц2 )
Fe Si Mn Ni PAl Cu As PbZn Sb Sn Impurity
2 - 4max   0.11 - 3max   0.5max   0.019 - 1181 - 88max   0.01max   0.3max   0.5max   0.05max   0.1 all 1
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrА10ZH3Mts2   ( БрА10Ж3Мц2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 493-79     490   12    
sand (mould) casting, GOST 493-79     392   10    


    Brinell hardness for     BrА10ZH3Mts2   ( БрА10Ж3Мц2 )   ,     cast in a metal mould GOST 493 HB 10 -1 = 120   MPa
    Brinell hardness for     BrА10ZH3Mts2   ( БрА10Ж3Мц2 )   ,     sand (mould) casting GOST 493 HB 10 -1 = 100   MPa


Friction coefficient of the material   BrА10ZH3Mts2   ( БрА10Ж3Мц2 ) .
 Friction coefficient with oil : 0.012


Technological properties of the material   BrА10ZH3Mts2   ( БрА10Ж3Мц2 ) .
        Melting temperature : 1045   °C
        Linear shrinkage : 2.4   %


Physical properties for grade   BrА10ZH3Mts2   ( БрА10Ж3Мц2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.98   58.6 7500   189
100   16        



Types of delivery of grade   BrА10ZH3Mts2   ( БрА10Ж3Мц2 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrА10ZH3Mts2   ( БрА10Ж3Мц2 ) - Tin-free foundary bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru