Characteristics for grade     BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 )



      Grade :     BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 )
      Classification :   Tin-free foundary bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 )
Fe Si Mn Ni PAl Cu As PbZn Sb Sn Impurity
4 - 5max   0.20.5 - 1.24 - 5max   0.038.8 - 1077.6 - 82.7max   0.05max   0.05max   1max   0.05max   0.2 all 1.2
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 493-79     587   12    
sand (mould) casting, GOST 493-79     587   12    


    Brinell hardness for     BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 )   ,     cast in a metal mould GOST 493 HB 10 -1 = 160   MPa
    Brinell hardness for     BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 )   ,     sand (mould) casting GOST 493 HB 10 -1 = 160   MPa


Equivalent steels for grade     BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 )
Warning! Indicated both exact and nearest equivalents.
USA
-
C95800




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrА9ZH4N4Mts1   ( БрА9Ж4Н4Мц1 ) - Tin-free foundary bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys