Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | NP3 ( НП3 ) |
Classification : | Semis nickel |
Equivalent grades: | Go here |
Grade NP3 ( НП3 ): supplier Auremo www.auremo.biz Sale: Russia +7 (812) 680-16-77 , Germany +49 (208) 376-298-00 , info [a] auremo.org |
Ni+Co | Fe | C | Si | Mn | S | Cu | Mg | Impurity |
min 99.3 | max 0.15 | max 0.15 | max 0.15 | max 0.2 | max 0.015 | max 0.15 | max 0.1 | all 0.7 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet hotrolled, GOST 6235-91 | 370 | 15 | ||||||
Sheet, GOST 6235-91 | 370 | 35 | ||||||
Sheet, GOST 6235-91 | 540 | 2 | ||||||
Bar hotrolled, GOST 13083-77 | 440 | 10 | ||||||
Bar, GOST 13083-77 | 370 | 30 | ||||||
Bar, GOST 13083-77 | 540 | 5 | ||||||
Band, GOST 2170-73 | 390 | 35 | ||||||
Band, GOST 2170-73 | 540 | 3 |
Melting temperature : | 1455 °C |
Forging temperature : | 1140 - 1250 °C |
Annealing temperature : | 700 - 800 °C |
Casting temperature : | 1550 - 1650 °C |
Linear shrinkage : | 1 % |
Germany | ||
DIN,WNr | ||
|
B34 - Ribbons |
B51 - Non-ferrous metals, including rare metals, and their alloys |
B53 - Sheets and Strips |
В54 - Ribbons |
B55 - Bars |
B74 - Wire made of non-ferrous metals and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2019 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. Previous address of this website was splav.kharkov.com |