Characteristics for grade     NK0.2   ( НК0.2 )



      Grade :     NK0.2   ( НК0.2 )
      Classification :   Nickel alloys
      Equivalent grades:     Is absent



Chemical composition in % for grade   NK0.2   ( НК0.2 )
Ni+Co Fe C Si Mn S P Cu As Pb Mg Zn Sb Bi Sn CdImpurity
min   99.4max   0.1max   0.10.15 - 0.25max   0.05max   0.005max   0.002max   0.1max   0.002max   0.002max   0.1max   0.007max   0.002max   0.002max   0.002max   0.002 all 0.45


Mechanical properties under Т=20oС for grade   NK0.2   ( НК0.2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 13083-77     540   5    
Bar, GOST 13083-77     370   30    
Bar hotrolled, GOST 13083-77     440   10    


    Brinell hardness for     NK0.2   ( НК0.2 )   ,     soft HB 10 -1 = 75   MPa
    Brinell hardness for     NK0.2   ( НК0.2 )   ,     hard HB 10 -1 = 190   MPa


Technological properties of the material   NK0.2   ( НК0.2 ) .
        Melting temperature : 1454   °C
        Forging temperature : 1150 - 850   °C
        Annealing temperature : 750 - 850   °C


Physical properties for grade   NK0.2   ( НК0.2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.17     8900   90
100   13.6        



Types of delivery of grade   NK0.2   ( НК0.2 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B55 - Bars
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  NK0.2   ( НК0.2 ) - Nickel alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru