Characteristics for grade     MNZHMts30-1-1   ( МНЖМц30-1-1 )



      Grade :     MNZHMts30-1-1   ( МНЖМц30-1-1 )
      Classification :   Copper-nickel alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   MNZHMts30-1-1   ( МНЖМц30-1-1 )
Ni+Co Fe C Si Mn S P Cu PbZn Impurity
29 - 330.5 - 1max   0.05max   0.150.5 - 1max   0.01max   0.0164.4 - 70max   0.05max   0.5 all 0.6
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   MNZHMts30-1-1   ( МНЖМц30-1-1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 10092-2006     350   35    
soft     350-450  40-50   
hard     550-650  3-5   


    Brinell hardness for     MNZHMts30-1-1   ( МНЖМц30-1-1 )   ,     soft HB 10 -1 = 58.8 - 68.9   MPa
    Brinell hardness for     MNZHMts30-1-1   ( МНЖМц30-1-1 )   ,     hard HB 10 -1 = 98   MPa


Technological properties of the material   MNZHMts30-1-1   ( МНЖМц30-1-1 ) .
        Melting temperature : 1230   °C
        Forging temperature : 860 - 950   °C
        Annealing temperature : 750 - 810   °C


Physical properties for grade   MNZHMts30-1-1   ( МНЖМц30-1-1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.45   37 8900   420
100   16        


Equivalent steels for grade     MNZHMts30-1-1   ( МНЖМц30-1-1 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapan
-DIN,WNrJIS
C71500
2.0882
CuNi30Mn1Fe
C7150



Types of delivery of grade   MNZHMts30-1-1   ( МНЖМц30-1-1 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  MNZHMts30-1-1   ( МНЖМц30-1-1 ) - Copper-nickel alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru