Grade : | NV3 ( НВ3 ) |
Classification : | Low- alloy nickel |
Equivalent grades: | Is absent |
Ni+Co | Fe | C | Si | Mn | S | P | W | Cu | As | Mg | Zn | Sb | Bi | Sn | Cd |
min 96 | max 0.07 | max 0.1 | max 0.02 | max 0.03 | max 0.005 | max 0.001 | 2.5 - 3.5 | max 0.05 | max 0.001 | max 0.05 | max 0.005 | max 0.001 | max 0.001 | max 0.001 | max 0.001 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Band, GOST 2170-73 | 540 | 3 | ||||||
Band, GOST 2170-73 | 390 | 35 |
В54 - Ribbons |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |