Characteristics for grade     MNZHMts10-1-1   ( МНЖМц10-1-1 )



      Grade :     MNZHMts10-1-1   ( МНЖМц10-1-1 )
      Classification :   Copper-nickel alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   MNZHMts10-1-1   ( МНЖМц10-1-1 )
Ni+Co Fe C Mn S Cu PbZn Impurity
9 - 111 - 2max   0.030.3 - 1max   0.0385.5 - 89.7max   0.03max   0.3 all 0.5
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   MNZHMts10-1-1   ( МНЖМц10-1-1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 10092-2006     290   35    
Pipe, GOST 10092-2006     420   5    


Physical properties for grade   MNZHMts10-1-1   ( МНЖМц10-1-1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       8900    


Equivalent steels for grade     MNZHMts10-1-1   ( МНЖМц10-1-1 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapan
-DIN,WNrJIS
C70600
2.0872
CuNi10Fe1Mn
C7060



Types of delivery of grade   MNZHMts10-1-1   ( МНЖМц10-1-1 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  MNZHMts10-1-1   ( МНЖМц10-1-1 ) - Copper-nickel alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru