YOU HERE:   Steel and Alloy   ->   Copper

Characteristics for grade     NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )



      Grade :   NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 ) (   Монель   )
      Classification :   Copper-nickel alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )
Ni+Co Fe C Si Mn S P Cu As Pb Mg Sb Bi Impurity
65.6 - 69.82 - 3max   0.2max   0.051.2 - 1.8max   0.01max   0.0127 - 29max   0.01max   0.003max   0.1max   0.002max   0.002 all 0.6
Comment: Ni+Co is a basis; the percentage of Ni+Co is given approximately.


Mechanical properties under Т=20oС for grade   NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 1525 - 91     490   20    
Bar, GOST 1525 - 91     440   35    
Band, GOST 5187-2003     570   4-6.5   
Band, GOST 5187-2003     440   22-25   
Strip, GOST 5063-73     440   25    
Strip, GOST 5063-73     570   6.5    


    Brinell hardness for     NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )   ,     soft HB 10 -1 = 135   MPa
    Brinell hardness for     NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )   ,     hard HB 10 -1 = 210   MPa


Technological properties of the material   NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 ) .
        Melting temperature : 1350   °C
        Forging temperature : 1170 - 920   °C
        Annealing temperature : 870 - 950   °C


Physical properties for grade   NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.82     8820   430
100   14        


Equivalent steels for grade     NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyFrancePolandCzechiaInter
-DIN,WNrAFNORPNCSNISO
04400
2.4361
LC-NiCu30Fe
NiCu30Fe
NiCu32Fe1.5Mn
NiCu30
Ni70Cu30
NiCu30



Types of delivery of grade   NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 )
B33 - Sheets and Strips
B51 - Non-ferrous metals, including rare metals, and their alloys
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  NMZHMts28-2.5-1.5   ( НМЖМц28-2.5-1.5 ) - Copper-nickel alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru