Characteristics for grade     А8   ( А8 )



      Grade :     А8   ( А8 )
      Classification :   Primary aluminium
      Equivalent grades:   Go here



Chemical composition in % for grade   А8   ( А8 )
Fe Si Mn TiAl Cu Mg Zn GaImpurity
max   0.12max   0.1max   0.02max   0.01min   99.8max   0.01max   0.02max   0.04max   0.03other, each 0.02;


Mechanical properties under Т=20oС for grade   А8   ( А8 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe annealed , GOST 18475-82     60   20    
Pipe cold-worked , GOST 18475-82     80   4-5   


Physical properties for grade   А8   ( А8 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2700    


Equivalent steels for grade     А8   ( А8 )
Warning! Indicated both exact and nearest equivalents.
USAEuropean
-EN
Aluminium1080
Aluminium1080A
ENAW-1080A



Types of delivery of grade   А8   ( А8 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  А8   ( А8 ) - Primary aluminium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys