Grade : | А7 ( А7 ) |
Classification : | Primary aluminium |
Equivalent grades: | Go here |
Fe | Si | Mn | Ti | Al | Cu | Mg | Zn | Ga | Impurity |
max 0.16 | max 0.15 | max 0.03 | max 0.01 | min 99.7 | max 0.01 | max 0.02 | max 0.04 | max 0.03 | other, each 0.02; |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe, GOST 18482-79 | 60 | 20 | ||||||
Band annealed , GOST 13726-97 | 60 | 20-30 | ||||||
Band cold-worked , GOST 13726-97 | 130-145 | 3-5 | ||||||
Plate , GOST 17232-99 | 64-78 | 15-18 |
Brinell hardness for А7 ( А7 ) , casted | HB 10 -1 = 20 MPa |
USA | Germany | Japan | European | Poland | Czechia | Inter | ||||||||||
- | DIN,WNr | JIS | EN | PN | CSN | ISO | ||||||||||
|
|
|
|
|
|
|
B51 - Non-ferrous metals, including rare metals, and their alloys |
B53 - Sheets and Strips |
В54 - Ribbons |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |