Grade : | А5 ( А5 ) |
Classification : | Primary aluminium |
Equivalent grades: | Go here |
Fe | Si | Mn | Ti | Al | Cu | Mg | Zn | Ga | Impurity |
max 0.3 | max 0.25 | max 0.05 | max 0.02 | min 99.5 | max 0.02 | max 0.03 | max 0.06 | max 0.03 | other, each 0.03; |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe, GOST 18482-79 | 60 | 20 | ||||||
Pipe cold-worked , GOST 18475-82 | 80 | 4-5 | ||||||
Band, GOST 13726-97 | 60 | 20-30 | Annealing | |||||
Band cold-worked , GOST 13726-97 | 130-145 | 3-5 | ||||||
Plate , GOST 17232-99 | 64-78 | 15-18 |
Brinell hardness for А5 ( А5 ) , casted | HB 10 -1 = 20 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 2700 |
USA | European | ||
- | EN | ||
|
|
B51 - Non-ferrous metals, including rare metals, and their alloys |
B53 - Sheets and Strips |
В54 - Ribbons |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |