Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Zinc

Characteristics for grade     TSV00   ( ЦВ00 )

      Grade :     TSV00   ( ЦВ00 )
      Classification :   Primary zinc
      Equivalent grades:     Is absent



Chemical composition in % for grade   TSV00   ( ЦВ00 )
Fe NiAl Cu As PbZn Sb Bi Sn CdImpurity
max   0.00001max   0.00001max   0.00001max   0.00001max   0.0005max   0.00001min   99.997max   0.00001max   0.00001max   0.00001max   0.002 all 0.003

Types of delivery of grade   TSV00   ( ЦВ00 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  TSV00   ( ЦВ00 ) - Primary zinc: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru