Characteristics for grade     TS0А   ( Ц0А )

      Grade :     TS0А   ( Ц0А )
      Classification :   Primary zinc
      Equivalent grades:     Is absent



Chemical composition in % for grade   TS0А   ( Ц0А )
FeAl Cu As PbZn Sn CdImpurity
max   0.003max   0.005max   0.001max   0.0005max   0.01min   99.98max   0.001max   0.003 all 0.02


Mechanical properties under Т=20oС for grade   TS0А   ( Ц0А )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
casted     120-140  0.3-0.530  
deformed     120-170  40-5060-80  


    Brinell hardness for     TS0А   ( Ц0А )   ,     casted HB 10 -1 = 30 - 40   MPa
    Brinell hardness for     TS0А   ( Ц0А )   ,     deformed HB 10 -1 = 35 - 45   MPa


Technological properties of the material   TS0А   ( Ц0А ) .
        Melting temperature : 419.5   °C
        Forging temperature : 150 - 170   °C
        Casting temperature : 430 - 450   °C
        Linear shrinkage : 1.57   %


Physical properties for grade   TS0А   ( Ц0А )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.95     7130    
100   39.5        

Types of delivery of grade   TS0А   ( Ц0А )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  TS0А   ( Ц0А ) - Primary zinc: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru