Characteristics for grade     16G2АF   ( 16Г2АФ )

      Grade :     16G2АF   ( 16Г2АФ )
      Substitute:   15Г2АФ, 14Г2АФ
      Classification :   Structural steel for welding construct
      Equivalent grades:   Go here



Chemical composition in % for grade   16G2АF   ( 16Г2АФ )
C Si Mn Ni S P Cr V N Cu As
0.14 - 0.20.3 - 0.61.3 - 1.7max   0.3max   0.035max   0.03max   0.40.08 - 0.140.015 - 0.025max   0.3max   0.08


Temperature of critical points for grade   16G2АF   ( 16Г2АФ ).
Ac1 = 723 ,      Ac3(Acm) = 907 ,       Mn = 400


Mechanical properties under Т=20oС for grade   16G2АF   ( 16Г2АФ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 19282-73 5 - 9   600 450 20    
Sheet to 50   510 390 19    


Technological properties for grade   16G2АF   ( 16Г2АФ )
  Weldability: without limitations.


Equivalent steels for grade     16G2АF   ( 16Г2АФ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandCanadaEuropeanItalySpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaSwitzerland
-DIN,WNrJIS AFNORBSHGEN UNIUNEGBSSBDSMSZPNSTASCSNSNV
A633Gr.E
K02002
K12202
K12437
1.8902
P460N
S420N
StE420
SM490A
SM490B
SM490C
SM490YA
SM490YB
STK540
E420RIFP
FeE420KGN
S420N
50E
50EE
S355NL
S420N
400WT
1.8902
S420N
FeE420KG
FeE420KW
AE420KG
S420N
Q420C
2143
09G2BFBFF
S420N
58C
E420D
S420N
18G2AV
K510
13220
StE43

Types of delivery of grade   16G2АF   ( 16Г2АФ )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  16G2АF   ( 16Г2АФ ) - Structural steel for welding construct: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru