Characteristics for grade     АDch   ( АДч )



      Grade :     АDch   ( АДч )
      Classification :   Technical aluminium
      Equivalent grades:   Go here



Chemical composition in % for grade   АDch   ( АДч )
Fe Si TiAl CuZn Impurity
max   0.03max   0.03max   0.002min   99.95max   0.015max   0.005other, each 0.005; all 0.05


Equivalent steels for grade     АDch   ( АДч )
Warning! Indicated both exact and nearest equivalents.
USA
-
AA1095




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АDch   ( АДч ) - Technical aluminium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru