Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | АD000 ( АД000 ) |
Classification : | Technical aluminium |
Equivalent grades: | Go here |
Fe | Si | Mn | Ti | Al | Cu | Mg | Zn | Impurity |
max 0.15 | max 0.15 | max 0.02 | max 0.02 | min 99.8 | max 0.03 | max 0.02 | max 0.06 | other, each 0.02; |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 2700 |
USA | Germany | Japan | France | England | European | Italy | Poland | Czechia | Austria | Inter | ||||||||||||||||||||||||
- | DIN,WNr | JIS | AFNOR | BS | EN | UNI | PN | CSN | ONORM | ISO | ||||||||||||||||||||||||
|
|
|
|
|
|
|
|
|
|
|
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |