Characteristics for grade     АD00   ( АД00 )



      Grade :   АD00   ( АД00 ) (   1010   )
      Classification :   Technical aluminium
      Equivalent grades:   Go here



Chemical composition in % for grade   АD00   ( АД00 )
Fe Si Mn TiAl Cu Mg Zn Impurity
max   0.25max   0.2max   0.03max   0.03min   99.7max   0.03max   0.03max   0.07other, each 0.02;


Mechanical properties under Т=20oС for grade   АD00   ( АД00 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 18482-79     60   20    
Band annealed , GOST 13726-97     60   20-30   
Band cold-worked , GOST 13726-97     130-145  3-5   
Plate , GOST 17232-99     64-78  15-18   


Physical properties for grade   АD00   ( АД00 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2700    


Equivalent steels for grade     АD00   ( АД00 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEuropeanItalySwedenPolandCzechiaAustriaInter
-DIN,WNrJIS AFNOREN UNISSPNCSNONORMISO
AA1070
AA1075
AA1170
AA1175
3.0275
Al99.7
1070
1070A
ENAW-1070A
ENAW-Al99.7
P-Al99.7
Al99.7
Al99.7
424003
Al99.7
1070A
Al99.7



Types of delivery of grade   АD00   ( АД00 )
B53 - Sheets and Strips
В54 - Ribbons
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АD00   ( АД00 ) - Technical aluminium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys