Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Aluminium alloy

Characteristics for grade     АD0E   ( АД0Е )



      Grade :   АD0E   ( АД0Е ) (   1011Е   )
      Classification :   Technical aluminium
      Equivalent grades:   Go here



Chemical composition in % for grade   АD0E   ( АД0Е )
Fe Si Mn Cr TiAl Cu BZn Impurity -
max   0.4max   0.1max   0.01max   0.01max   0.05min   99.5max   0.05max   0.05max   0.05other, each 0.03; all 0.1 V+Ti < 0.02


Physical properties for grade   АD0E   ( АД0Е )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2710    


Equivalent steels for grade     АD0E   ( АД0Е )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanEnglandEuropeanSwedenPolandCzechiaAustriaInter
-DIN,WNrJIS BSEN SSPNCSNONORMISO
AA1050
AA1055
AA1060
AA1065
3.0255
Al99.5
E-AI
1050
1350
AWEAI99,5
ENAW-1050A
ENAW-Al99.5
EAI99,5
AI99,5E
424003
E-AI
1350
EA199.5




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АD0E   ( АД0Е ) - Technical aluminium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru