Characteristics for grade     АD1   ( АД1 )



      Grade :   АD1   ( АД1 ) (   1013   )
      Classification :   Technical aluminium
      Equivalent grades:   Go here



Chemical composition in % for grade   АD1   ( АД1 )
Fe Si Mn TiAl Cu Mg Zn Impurity
max   0.3max   0.3max   0.025max   0.15min   99.3max   0.05max   0.05max   0.1other, each 0.05;


Mechanical properties under Т=20oС for grade   АD1   ( АД1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 18482-79     60   20    
Pipe annealed , GOST 18475-82     60-110  20    
Pipe cold-worked , GOST 18475-82     100-110  4-5   
Bar, GOST 21488-97     60   25    
Band cold-worked , GOST 13726-97     130-145  3-5   
Band annealed , GOST 13726-97     60   20-30   
Profile, GOST 8617-81     59   20    
Profile cold-worked , GOST 18591-91     98        


Physical properties for grade   АD1   ( АД1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.71     2710   29.2
100   24 226      
200   25.6        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     АD1   ( АД1 )
Warning! Indicated both exact and nearest equivalents.
USAEuropeanInter
-EN ISO
AA1135
AA1145
AA1230
AA1235
AA1345
ENAW-1235
ENAW-Al99.35
A199.3



Types of delivery of grade   АD1   ( АД1 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B52 - Graded and shaped rolling
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АD1   ( АД1 ) - Technical aluminium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru