Characteristics for grade     TSam10-5   ( Цам10-5 )

      Grade :     TSam10-5   ( Цам10-5 )
      Classification :   Zinc antifriction alloys
      Equivalent grades:     Is absent



Chemical composition in % for grade   TSam10-5   ( Цам10-5 )
Fe Si Al Cu Pb Mg Zn Sn CdImpurity
max   0.15max   0.19 - 124 - 5.5max   0.030.03 - 0.0681.8 - 86.62max   0.01max   0.02 all 0.35
Comment: Zn is a basis; the percentage of Zn is given approximately.


Mechanical properties under Т=20oС for grade   TSam10-5   ( Цам10-5 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
 , GOST 21437-95     343   4    


    Brinell hardness for     TSam10-5   ( Цам10-5 )   ,       GOST 21437-95 HB 10 -1 = 90   MPa


Limiting operating condition of the material   TSam10-5   ( Цам10-5 )
Load Speed Load * Speed Temperature
MPa m/s MPa * m/s Grade
19.68   80


Technological properties of the material   TSam10-5   ( Цам10-5 ) .
        Melting temperature : 378 - 395   °C
        Linear shrinkage : 1   %


Physical properties for grade   TSam10-5   ( Цам10-5 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.9   100.8 6300    
100   27        

Types of delivery of grade   TSam10-5   ( Цам10-5 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  TSam10-5   ( Цам10-5 ) - Zinc antifriction alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru