Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Titanium

Characteristics for grade     VT1-1   ( ВТ1-1 )



      Grade :     VT1-1   ( ВТ1-1 )
      Classification :   Titanium
      Equivalent grades:     Is absent



Chemical composition in % for grade   VT1-1   ( ВТ1-1 )
Fe C Si N Ti OH Impurity
max   0.25max   0.08max   0.12max   0.0599.038 - 99.7max   0.15max   0.012 other 0.3
Comment: Ti is a basis; the percentage of Ti is given approximately.


Mechanical properties under Т=20oС for grade   VT1-1   ( ВТ1-1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
      450-600380-50025 50  


    Brinell hardness for     VT1-1   ( ВТ1-1 )   ,       HB 10 -1 = 131 - 163   MPa


Technological properties for grade   VT1-1   ( ВТ1-1 )
  Weldability: without limitations.


Technological properties of the material   VT1-1   ( ВТ1-1 ) .
        Melting temperature : 1668   °C


Physical properties for grade   VT1-1   ( ВТ1-1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.12   18.85 4505 540  
100   8.2        




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  VT1-1   ( ВТ1-1 ) - Titanium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru