Characteristics for grade     OT4-1   ( ОТ4-1 )



      Grade :     OT4-1   ( ОТ4-1 )
      Classification :   Titanium wrought alloy
      Equivalent grades:   Go here



Chemical composition in % for grade   OT4-1   ( ОТ4-1 )
Fe C Si Mn N TiAl Zr OH Impurity
max   0.3max   0.1max   0.120.7 - 2max   0.0594.33 - 97.51.5 - 2.5max   0.3max   0.15max   0.012 other 0.3
Comment: Ti is a basis; the percentage of Ti is given approximately.


Mechanical properties under Т=20oС for grade   OT4-1   ( ОТ4-1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet annealed , GOST 22178-76     590   13-25   
Bar, GOST 26492-85 Ø 10 - 150   540   10-1221-30400-450Annealing
Bar, GOST 26492-85     540-735  13-1524-35400-450Annealing
Plate , GOST 23755-79 11 - 150   590-735  8-1014-18  


    Brinell hardness for     OT4-1   ( ОТ4-1 )   ,       HB 10 -1 = 197 - 255   MPa


Technological properties for grade   OT4-1   ( ОТ4-1 )
  Weldability: without limitations.


Physical properties for grade   OT4-1   ( ОТ4-1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.1   9.63 4550   1010
100   8 10.47      
200   8 11.3   0.565  
300   9.1 12.14   0.628  
400   9.6 14.24   0.67  
500   9.7 14.65   0.754  
600   9.8 16.32      
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     OT4-1   ( ОТ4-1 )
Warning! Indicated both exact and nearest equivalents.
Japan
JIS
ST-A90



Types of delivery of grade   OT4-1   ( ОТ4-1 )
B53 - Sheets and Strips
B55 - Bars
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  OT4-1   ( ОТ4-1 ) - Titanium wrought alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru