Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Titanium

Characteristics for grade     VT14   ( ВТ14 )



      Grade :     VT14   ( ВТ14 )
      Classification :   Titanium wrought alloy
      Equivalent grades:   Go here



Chemical composition in % for grade   VT14   ( ВТ14 )
Fe C Si Mo V N TiAl Zr OH Impurity
max   0.25max   0.1max   0.152.5 - 3.80.9 - 1.9max   0.0586.85 - 92.83.5 - 6.3max   0.3max   0.15max   0.015 other 0.3
Comment: Ti is a basis; the percentage of Ti is given approximately.


Mechanical properties under Т=20oС for grade   VT14   ( ВТ14 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 22178-76     1080-1180  4-6  Quenching and artificial aging
Sheet, GOST 22178-76     835-885  8   Annealing
Bar, GOST 26492-85     1080   4 8200Hardening and ageing
Bar, GOST 26492-85     865-1080  8-1025-35450-500Annealing
Bar, GOST 26492-85     865-1080  8-1025-35450-500Annealing
Bar, GOST 26492-85     1080   4-68-12200-250Hardening and ageing
Die     850-900  10-15  Annealing
Die     1250-1300  6-1520-40500Hardening and ageing
Plate annealed , GOST 23755-79 11 - 100   835-1030  6-714-20  


    Brinell hardness for     VT14   ( ВТ14 )   (annealing) ,     Die HB 10 -1 = 255 - 341   MPa
    Brinell hardness for     VT14   ( ВТ14 )   (quenching, ageing) ,     Die HB 10 -1 = 302 - 388   MPa


Technological properties for grade   VT14   ( ВТ14 )
  Weldability: without limitations.


Physical properties for grade   VT14   ( ВТ14 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.1   8.37 4520    
100   8 9.21      
200   8.2 10.47   0.544  
300   8.5 11.72   0.586  
400   8.8 12.92   0.628  
500   8.9 13.82   0.67  
600   8.7     0.712  
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     VT14   ( ВТ14 )
Warning! Indicated both exact and nearest equivalents.
USAFrance
-AFNOR
4Al-3Mo-1V
T-A4D3V



Types of delivery of grade   VT14   ( ВТ14 )
B53 - Sheets and Strips
B55 - Bars
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  VT14   ( ВТ14 ) - Titanium wrought alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys