Grade : | АL3 ( АЛ3 ) |
Classification : | Aluminium casting alloys |
Equivalent grades: | Go here |
Fe | Si | Mn | Al | Cu | Pb | Mg | Zn | Sn | Impurity | - |
max 1.6 | 4.5 - 5.5 | 0.6 - 0.9 | 88.1 - 93.05 | 1.5 - 3 | max 0.05 | 0.35 - 0.6 | max 0.3 | max 0.01 | all 1.9 | Zr+Ce<0.5 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
cast in a metal mould | 270 | 200 | 1.5 | |||||
sand (mould) casting | 250 | 170 | 1 |
Brinell hardness for АL3 ( АЛ3 ) , cast in a metal mould | HB 10 -1 = 85 MPa |
Brinell hardness for АL3 ( АЛ3 ) , sand (mould) casting | HB 10 -1 = 80 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.7 | 2700 | 44.9 | |||
100 | 22 | 163 | 920 |
Japan | China | |||
JIS | GB | |||
|
|
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |