Grade : | АK9pch ( АК9пч ) ( АЛ4-1 ) |
Classification : | Aluminium casting alloys |
Equivalent grades: | Go here |
Fe | Si | Mn | Ti | Al | Cu | Zr | B | Pb | Be | Mg | Zn | Sn | Impurity |
max 0.3 | 9 - 10.5 | 0.2 - 0.35 | 0.08 - 0.15 | 87.62 - 90.49 | max 0.1 | max 0.15 | max 0.1 | max 0.03 | max 0.1 | 0.23 - 0.3 | max 0.3 | max 0.005 | all 0.6 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
cast in a metal mould, GOST 1583-93 | 157 | 3 | ||||||
cast in a metal mould, GOST 1583-93 | 265 | 4 | Quenching and artificial aging |
Brinell hardness for АK9pch ( АК9пч ) , GOST 1583-93 | HB 10 -1 = 50 - 70 MPa |
USA | |
- | |
|
B51 - Non-ferrous metals, including rare metals, and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |