Characteristics for grade     АK7   ( АК7 )



      Grade :   АK7   ( АК7 ) (   АЛ9В   )
      Classification :   Aluminium casting alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   АK7   ( АК7 )
Fe Si Mn NiAl Cu Mg Zn Impurity
max   1.36 - 80.2 - 0.6max   0.387.6 - 93.6max   1.50.2 - 0.5max   0.5 all 3.3
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   АK7   ( АК7 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 1583-93     127-196  0.5-1   


    Brinell hardness for     АK7   ( АК7 )   ,     Casting GOST 1583-93 HB 10 -1 = 50 - 75   MPa


Equivalent steels for grade     АK7   ( АК7 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyChinaSwedenPolandCzechia
-DIN,WNrJIS AFNORBSEN UNIGBSSPNCSN
356
357.0
A03560
G-AlSi12(Cu)
G—AlSi7Mg
AC4В
A-S10G
A-S7G
LM25
ENAC-42000
ENAC-AlSi7Mg
GAISi7Mg
HZL101
ZL101
ZL11
AISi7MgFe
AISi7Mg
424332



Types of delivery of grade   АK7   ( АК7 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АK7   ( АК7 ) - Aluminium casting alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru