Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Tool steel

Characteristics for grade     KHV4F   ( ХВ4Ф )

      Grade :     KHV4F   ( ХВ4Ф )
      Classification :   Alloy tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   KHV4F   ( ХВ4Ф )
C Si Mn Ni S P Cr Mo W V Cu
1.25 - 1.450.15 - 0.350.15 - 0.4max   0.35max   0.03max   0.030.4 - 0.7max   0.53.5 - 4.30.15 - 0.3max   0.3


Temperature of critical points for grade   KHV4F   ( ХВ4Ф ).
Ac1 = 750 - 760


    Brinell hardness for     KHV4F   ( ХВ4Ф )   (annealing) ,       HB 10 -1 = 255   MPa


Technological properties for grade   KHV4F   ( ХВ4Ф )
  Weldability: is not used.
Temper brittleness: weakly predisposed


Equivalent steels for grade     KHV4F   ( ХВ4Ф )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanCzechiaAustria
-DIN,WNrJIS CSNONORM
F2
X130W5
SKS11
19714
K400


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  KHV4F   ( ХВ4Ф ) - Alloy tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)