Characteristics for grade     AMg5K   ( АМг5К )



      Grade :   AMg5K   ( АМг5К ) (   АЛ13   )
      Classification :   Aluminium casting alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   AMg5K   ( АМг5К )
Fe Si Mn Al Cu Zr Mg Zn Impurity
max   1.50.8 - 1.30.1 - 0.491 - 94.6max   0.1max   0.154.5 - 5.5max   0.2 all 1.8
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   AMg5K   ( АМг5К )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
 , GOST 1583-93     147-167  0.5-1   


    Brinell hardness for     AMg5K   ( АМг5К )   ,       GOST 1583-93 HB 10 -1 = 55   MPa


Technological properties of the material   AMg5K   ( АМг5К ) .
        Linear shrinkage : 1.2   %


Physical properties for grade   AMg5K   ( АМг5К )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20   20        


Equivalent steels for grade     AMg5K   ( АМг5К )
Warning! Indicated both exact and nearest equivalents.
USAGermanyFranceEnglandEuropeanChinaSwedenPolandCzechiaInter
-DIN,WNrAFNORBSEN GBSSPNCSNISO
512.0
A25140
G-AlMg5
G-AlMg5Si
GK-AlMg5
A-G6
LM5
AC-AlMg5Si
ZAlMg5Si1
ZL303
AlMg5Si
AlMg5Si1
424515
AlMg5Si1



Types of delivery of grade   AMg5K   ( АМг5К )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  AMg5K   ( АМг5К ) - Aluminium casting alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru