Characteristics for grade     AK13MMgN   ( АК12ММгН )



      Grade :   AK13MMgN   ( АК12ММгН ) (   АЛ30   )
      Classification :   Aluminium casting alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   AK13MMgN   ( АК12ММгН )
Fe Si Mn Ni Cr TiAl Cu Pb Mg Zn Sn Impurity
max   0.711 - 13max   0.20.8 - 1.3max   0.2max   0.282.64 - 86.60.8 - 1.5max   0.050.8 - 1.3max   0.2max   0.01 all 1.1
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   AK13MMgN   ( АК12ММгН )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 1583-93     196-216  0.5-0.7  Ageing


    Brinell hardness for     AK13MMgN   ( АК12ММгН )   ,     cast in a metal mould GOST 1583-93 HB 10 -1 = 90 - 100   MPa


Technological properties of the material   AK13MMgN   ( АК12ММгН ) .
        Casting temperature : 700   °C
        Linear shrinkage : 1.15   %


Physical properties for grade   AK13MMgN   ( АК12ММгН )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2700    
100   19        


Equivalent steels for grade     AK13MMgN   ( АК12ММгН )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandChinaInter
-DIN,WNrJIS AFNORBSGBISO
383
A03360
A13320
G-AlSi12(Cu)
GK-AlSi12(Cu)
AC8A
A-S11UNG
A-S12UNG
A-S9GU
A—S12UN
LM13
ZAlSi12Cu1Mg1Ni1
ZL109
AlSi12Cu



Types of delivery of grade   AK13MMgN   ( АК12ММгН )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  AK13MMgN   ( АК12ММгН ) - Aluminium casting alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru