Characteristics for grade     АMg1   ( АМг1 )



      Grade :   АMg1   ( АМг1 ) (   1510   )
      Classification :   Aluminium wrought alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   АMg1   ( АМг1 )
Fe Si Mn CrAl Cu Mg Zn Impurity
max   0.7max   0.3max   0.2max   0.197.15 - 99.5max   0.20.5 - 1.1max   0.25other, each 0.05; all 0.15
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   АMg1   ( АМг1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe annealed , GOST 18475-82     120-175  10    
Pipe cold-worked , GOST 18475-82     165        


Technological properties for grade   АMg1   ( АМг1 )
  Weldability: without limitations.


Physical properties for grade   АMg1   ( АМг1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2690    


Equivalent steels for grade     АMg1   ( АМг1 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceItalyInter
-DIN,WNrJIS AFNORUNIISO
AA5005
AA5006
3.3315
AlMg1
5005
A-G0.6
P-AlMg0.9
5005
AlMg1



Types of delivery of grade   АMg1   ( АМг1 )
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  АMg1   ( АМг1 ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys