Chemical composition in % for grade   АMg4.5   ( АМг4.5 )
Fe Si Mn Cr TiAl Cu Be Mg Zn Impurity
max   0.4max   0.40.4 - 10.05 - 0.25max   0.1592.545 - 95.55max   0.1max   0.0054 - 4.9max   0.25other, each 0.05; all 0.15
Comment: Al is a basis; the percentage of Al is given approximately.


Physical properties for grade   АMg4.5   ( АМг4.5 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2660    


Equivalent steels for grade     АMg4.5   ( АМг4.5 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySwedenPolandCzechiaAustriaInter
-DIN,WNrJIS AFNORBSEN UNISSPNCSNONORMISO
A95083
3.3547
AIMg4.5
5082
5083
5183
5083
ENAW-5083
ENAW-5086
ENAW-AlMg4
ENAW-AlMg4.5Mn0.7
PAIMg4.4
AIMg4.5Mn
AIMg4.5Mn
424415
AIMg4.5Mn
5083
AlMg4.5




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АMg4.5   ( АМг4.5 ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru