Grade : | V95P ( В95П ) ( 1957 ) |
Classification : | Aluminium wrought alloys |
Equivalent grades: | Is absent |
Fe | Si | Mn | Cr | Al | Cu | Mg | Zn | Impurity |
max 0.3 | max 0.3 | 0.3 - 0.5 | 0.1 - 0.25 | 87.45 - 90.7 | 1.4 - 2 | 2 - 2.6 | 5.5 - 6.5 | other, each 0.05; all 0.1 |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |