Grade : | АMg5P ( АМг5П ) ( 1557 ) |
Classification : | Aluminium wrought alloys |
Equivalent grades: | Is absent |
Fe | Si | Mn | Al | Cu | Mg | Impurity |
max 0.4 | max 0.4 | 0.2 - 0.6 | 92.6 - 95.1 | max 0.2 | 4.7 - 5.7 | other, each 0.05; all 0.1 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Wire | 270 | 150 | 23 |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.71 | 2650 | 62.5 | |||
100 | 24.1 | 126 | 922 |
B74 - Wire made of non-ferrous metals and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |