Grade : | АMg2 ( АМг2 ) ( 1520 ) |
Classification : | Aluminium wrought alloys |
Equivalent grades: | Go here |
Fe | Si | Mn | Cr | Ti | Al | Cu | Mg | Zn | Impurity |
max 0.5 | max 0.4 | 0.1 - 0.5 | max 0.05 | max 0.15 | 95.7 - 98.2 | max 0.15 | 1.7 - 2.4 | max 0.15 | other, each 0.05; all 0.15 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe, GOST 18482-79 | 155 | 60 | 10 | |||||
Bar, GOST 21488-97 | 175 | 13 | ||||||
Band, GOST 13726-97 | 175 | 7 | ||||||
Band cold-worked , GOST 13726-97 | 265-215 | 3-4 | ||||||
Profile annealed , GOST 8617-81 | 225 | 59 | 13 | |||||
Profile, GOST 8617-81 | 147 | 59 | 13 | |||||
Plate , GOST 17232-99 | 155-175 | 6-7 |
Brinell hardness for АMg2 ( АМг2 ) , | HB 10 -1 = 45 MPa |
Brinell hardness for АMg2 ( АМг2 ) (cold-worked) , | HB 10 -1 = 60 MPa |
Weldability: | without limitations. |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.71 | 2690 | 47.6 | |||
100 | 24.2 | 159 | 963 | |||
200 | 27.6 | |||||
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
USA | Germany | Japan | France | England | European | Italy | Sweden | Poland | Czechia | Austria | Inter | |||||||||||||||||||||
- | DIN,WNr | JIS | AFNOR | BS | EN | UNI | SS | PN | CSN | ONORM | ISO | |||||||||||||||||||||
|
|
|
|
|
|
|
|
|
|
|
|
B51 - Non-ferrous metals, including rare metals, and their alloys |
B52 - Graded and shaped rolling |
B53 - Sheets and Strips |
В54 - Ribbons |
B55 - Bars |
B64 - Pipes of non-ferrous metals and alloys |
B74 - Wire made of non-ferrous metals and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
Weldability : | |
without limitations | - welding is done without heating and subsequent heat treeting |
limited weldability | - welding is possible under heating up to 100-120 grade and subsequent heat treeting |
hard weldability | - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing |